Zinc Oxide doped with Scandia Sputtering Targets (ZnO/Sc2O3 98/02 wt%)
Material Type | Zinc Oxide doped with Scandia |
Symbol | ZnO / Sc2O3, 98 / 2 wt% |
Color/Appearance | Various colors, Solid |
Melting Point (°C) | N/A |
Relative Density (g/cc) | >95% |
Water Solubility | Insoluble |
Sputter | RF, RF-R, DC |
Type of Bond | Indium, Elastomer |
Comments | Various composition available |
Zinc Oxide doped with Scandia Sputtering Targets
ZnO is promising for a number of applications in light emission, sensors, and transparent conducting electronics, but its surface is susceptible to instabilities caused by atmospheric exposure. Thus, there is a need for stable passivation or gate dielectric layers that might obviate this issue. One potential candidate is Sc2O3.
Zinc Oxide doped with Scandia Sputtering Targets Information
Zinc Oxide doped with Scandia Sputtering Targets
Purity: 99.9%;
Circular: Diameter <= 14 inch, Thickness >= 1mm;
Block: Length <= 32 inch, Width <= 12 inch, Thickness >= 1mm.
More Information on Zinc Oxide doped with Scandia Sputtering Targets
Applications• Ferroelectric• Gate Dielectric • For CMOS |
Features• High purity• Custom sizes available |
Manufacturing Process• Manufacturing - Cold pressed - Sintered, Elastomer bonded to backing plate
• Cleaning and final packaging, Cleaned for use in vacuum, |
Options
• 99.9% minimum purity
• Smaller sizes also available for R&D applications
• Sputtering target bonding service
|
Related Products of Zinc Oxide doped with Scandia Sputtering Targets
Ceramic Sputtering Targets |
||
Evaporation Materials |
Crucibles N/A |
Metal Powders Zinc Powder |
Click to download datasheet about Zinc Oxide doped with Scandia Sputtering Targets (ZnO/Sc2O3 98/02 wt%)
Unable to find the required data sheet? Click here to send an email and get it.
Click here to get answers to Frequently Asked Questions (FAQ).
Related Products
FREE QUOTE